Product Features
UC-2210 resin is a polycarbonate-modified polyurethane dispersion. The product has good chemical resistance and outstanding water resistance. It has good adhesion to difficult-to-adhere nylon substrates, good flexibility, and excellent weather resistance.

Application
Good flexibility and good adhesion with metal, nylon, ABS, PC and other plastics. Used for automotive repair paint for large vehicles, industrial metal paint, one-component baking paint, two-component paint, etc.

Product Performance
Good weather resistance, high wear resistance; good fullness, high gloss; excellent chemical resistance

Product Specifications

Physical properties

Value

Appearance

Milk white Liquid

Organic solvent

0

Non-volatile components%

35

Neutralizer

DEMEA

PH

7.5 -8

Save
Please store it in a cool and dry place away from light. The storage temperature should be between 5 and 30°C. Keep the packaging intact. The shelf life of this product is 6 months from the production date. Performance evaluation before use over 6 months. This product needs to be strictly protected from frost, rain andtext-align:center">5

Go Ionized water

33.1

6

DMEA

BASF

0.3 -1

7

RM -8W

Luo Menhas

0.3

Total

100

Full proportion

lacquer : Cross-linking agent; Deionized water=20: 1: 5--8


Craftsmanship
1. Put 1. into a clean jar, slowly add parts 2 and 3, and stir evenly at low speed
2. Add 5. deionized water and stir evenly
3. Use 6 parts to adjust the pH to 7.5-8.5
4. Add part 7 and stir for 30 minutes
5. Add part 4 and mix well
6. If submitted for inspection, filtered and packaged.

Notes
1. When preparing the paint liquid, be sure to stir the cross-linking agent and the paint liquid evenly first, then add deionized water, stir well, and leave it for 10 minutes before use
2. When baking, please bake at a low temperature of 60-80°C for 3-5 minutes, and then bake at a high temperature to prevent bubbles from being generated by the intense reaction
3. Please prepare the paint for immediate use and do not leave it overnight. Unused paint cannot be poured into the original paint bucket
This formula is only used as a reference and is subject to actual performance requirements.

广告位
This article is from the Internet, does not represent the position of Epoxy curing agent, reproduced please specify the source.https://www.dmp-30.vip/archives/63725

author:

Previous article
Next article
Contact Us

Contact us

+86 - 152 2121 6908

Online consultation: QQ交谈

E-mail: info@newtopchem.com

Working hours: Monday to Friday, 9:00-17:30, closed on holidays
Follow wechat
Scan wechat and follow us

Scan wechat and follow us

Follow Weibo
Back to top
Home
Phone
Products
Search